Rockwell–Rockwell Superficial–Brinell–Vickers–Shore Hardness Conversion Chart
Rockwell |
||||||
| Hardness Scale | Symbol | Indenter Type | Load | Typical Range | Equivalent Standards | Best for Materials |
| • Rockwell A | HRA | 120° diamond cone (Brale) | 60 kgf | 70-95 HRA | ISO 6508, ASTM E18 | Tungsten carbide, thin case hardening |
| • Rockwell B | HRB | 1/16″ (1.588mm) steel ball | 100 kgf | 40-100 HRB | ISO 6508, ASTM E18 | Annealed steels, aluminum alloys |
| • Rockwell C | HRC | 120° diamond cone (Brale) | 150 kgf | 20-70 HRC | ISO 6508, ASTM E18 | Hardened tool steels (P20, H13) |
| • Rockwell D | HRD | 120° diamond cone (Brale) | 100 kgf | 40-80 HRD | ISO 6508, ASTM E18 | Thin hard coatings |
| • Rockwell E | HRE | 1/8″ (3.175mm) steel ball | 100 kgf | 70-100 HRE | ISO 6508, ASTM E18 | Soft metals (copper, brass) |
| • Rockwell F | HRF | 1/16″ (1.588mm) steel ball | 60 kgf | 60-100 HRF | ISO 6508, ASTM E18 | Annealed non-ferrous alloys |
Rockwell Superficial |
||||||
| • 15-N | HR15N | 120° diamond cone (Brale) | 15 kgf | 70-94 HR15N | ASTM E18 | Nitrided surfaces, thin sections |
| • 30-N | HR30N | 120° diamond cone (Brale) | 30 kgf | 40-90 HR30N | ASTM E18 | Case-hardened layers |
| • 45-N | HR45N | 120° diamond cone (Brale) | 45 kgf | 20-80 HR45N | ASTM E18 | Medium-depth hardened zones |
| • 30-T | HR30T | 1/16″ (1.588mm) steel ball | 30 kgf | 40-80 HR30T | ASTM E18 | Zinc alloys, soft steels |
Brinell |
||||||
| • Standard | HB | 10mm tungsten carbide ball | 3000 kgf | 100-650 HB | ISO 6506, ASTM E10 | Mold bases, ductile metals |
| • Light Load | HB | 10mm steel ball | 500 kgf | 30-200 HB | ISO 6506, ASTM E10 | Soft metals (aluminum, copper) |
| Vickers | HV | 136° diamond pyramid | 1-120 kgf | 50-3000 HV | ISO 6507, ASTM E384 | Micro-hardness, coatings |
Shore |
||||||
| • Shore D | HS D | Spring-loaded cone | N/A | 50-90 HS D | ISO 868, ASTM D2240 | Rigid plastics, polyurethane |
| • Shore C | HS C | Spring-loaded cone | N/A | 20-90 HS C | ISO 7619 | Elastomers, soft rubbers |
| Scleroscope | HS | Diamond-tipped hammer | Dynamic rebound | 20-140 HS | ASTM A956 | Large mold components (field testing) |
Factory Overview
Latest Post
Injection Mold Materials Commonly Used in the Automotive Industry
5 Points To Extend The Service Life Of Plastic Injection Mold
How To Optimize Injection Mold To Reduce Production Cycles?
How To Choose The Right Mold Supplier In The Automotive Industry?
Call
+86-0769-86066062
info@kehuimold.com
Service Time
9:00 AM – 10:00 PM